Furnace tubes face heat, carburisation and thermal fatigue. This guide covers alloy grades, failure modes, and coil versus single-tube replacement.
A cracking or process furnace is a bundle of tubes first and a steel box second. The radiant coils sit in the firebox, where the feed is heated to cracking temperature; the convection bundles above them recover heat from the flue gas; pigtails connect the coil outlets to the outlet manifold, and crossover piping carries the cracked gas on to the next step of the plant. Each of these parts sees a different temperature and a different duty, so they are specified as separate items, not as one generic tube.
Our supply covers the whole tube circuit of the furnace: radiant coils for ethylene crackers, convection bundles including finned and studded tubes, pigtails, outlet manifolds and crossover piping, plus reformer tubes and fired-heater bundles. Because the cracked gas leaving the furnace is quenched downstream in a Quench / Transfer-Line Exchangers (TLE), the outlet manifold and the pigtails must match the quench exchanger's inlet conditions as well as the furnace's own duty.
The alloy grade is the first decision, and it is made from the service temperature. The grades most often specified for radiant service are HP40, HT and HK40, together with Nb/Ti-modified grades; the same families are used for the associated pigtails and manifolds so the whole high-temperature circuit ages at a similar rate. In the data we supply, service temperature for these alloys runs up to approximately 1150 °C, and the grade must be chosen against the actual tube-metal temperature of the furnace, not against the process gas temperature alone.
A second decision is the manufacturing route. Our tubes are centrifugally cast — the process that gives a dense, uniform wall in high-temperature alloys — followed by machining and welding into coils, pigtails and manifolds. Each tube is inspected before shipment, and the inspection package can be agreed with the buyer in advance: radiographic testing (RT), penetrant testing (PT), dimensional checks and material verification (PMI) are the standard items listed on the product page.
Furnace tubes do not usually fail suddenly; they degrade over years. The three mechanisms named on the product page are sustained high temperature, carburisation and thermal fatigue. Carburisation hardens and embrittles the inner wall as carbon diffuses into the alloy; thermal fatigue opens cracks where the metal is cycled between hot and less hot states; and long exposure at high temperature slowly changes the alloy structure itself. Any one of these shortens furnace run length, and together they are the reason tube condition is watched, not assumed.
Material and fabrication quality directly sets furnace run length and safety, which is why this article keeps coming back to grade and inspection. A tube that has lost ductility to carburisation can fail during a shutdown or a restart, when thermal stresses peak — so the interesting question is not only which alloy was installed, but how much of its life is left. That is what the next section is about: measuring, not guessing.
When tubes reach the end of their life, there are two ways to replace them: a complete coil, or single tubes. A complete coil is the cleaner option when the whole radiant section has aged together — the new coil is built to the original drawings or reverse-engineered from the existing tubes and installed as one assembly. Single-tube replacement suits the case where only a few tubes show damage and the rest of the coil still has life; it costs less in material but leaves a mixed-age coil, so it pays only when the remaining tubes are known to be sound.
That judgement comes from tube mapping and remaining-life assessment. Mapping records the condition of every tube in the coil; the remaining-life assessment combines those readings with the service history to say which tubes stay and which go. The same service covers pigtails, manifolds and spares, so a shutdown can be planned around a measured list — tubes to replace, spares to have on site — instead of a guess made after the furnace is opened.
The last step before delivery is proving the tubes are what they claim to be. Centrifugally cast tubes are machined to size, welded into the required configuration, and then checked: RT and PT for the welds and cast structure, dimensional checks against the drawing, and PMI to confirm the alloy grade on the finished tube rather than on a mill certificate alone. These checks are listed on the product page as the standard inspection scope, and additional items can be agreed before manufacture starts.
Ordering is the same route as for the rest of the furnace circuit: tubes can be supplied from the buyer's own drawings, reverse-engineered from a sample or from measurements taken on the installed coil, or redesigned for new process conditions. Welding and installation support is part of the delivery — tube welding is where a good casting becomes a good coil or a leak — and the related equipment downstream, for example the Heat Exchangers in the convection and heat-recovery sections, can be specified in the same enquiry.
Further reading: Steam cracking — Wikipedia